I have questions and comments. 1 when you need to so called drill out the spot weld with the glued on panel how do you do it?
Do you use heat to release it?
2 Comment; even if the glue is using a molecular bond, there is only so much unit area, meaning a very thin penetration into the material its bonding. If the weld covered the same area as the glue did the weld will way surpass the glue.
3 Comment; a good welded panel can be made to look like it wasn't repaired, you could never do that with glue. I'm talking before putting any sort of paint on the bare metal.


Kicking self for selling off my Taskforce trucks.
Still looking for an LCF or conventional big bolt in decent shape.


As of 10-26-2022, A 55.2 Taskforce long bed now the work begins