I just did my frame with phosphoric acid, the "metal prep" for POR-15. I sprayed it on, let it set for 10-15 minutes, keeping it wet, then rinsed. The result looks splotchy, although it feels even. Is that normal? It does feel like it gave some tooth to the metal that had been smooth. Should it appear as an even coat or does that even matter?