The Stovebolt.com Forums Home | Tech Tips | Gallery | FAQ | Events | Features | Search
Help is a click away!

VEHICLE
INFORMATION
KITS


at the

GM Heritage Center
All the details are here.

Searching the Site - a click away
click here to search
New here ??? Where to start?
Click on image for the lowdown. Where do I go around here?
====
Who's Online Now
3 members (tclederman, TUTS 59, 1 invisible), 132 guests, and 1 robot.
Key: Admin, Global Mod, Mod
Forum Statistics
Forums66
Topics128,113
Posts1,056,279
Members48,439
Most Online14,466
Apr 26th, 2026
Step-by-step instructions for pictures in the forums
Brad Allen's photos

AD Chevy Trucks

Pictures galore
Over 6,000 pictures

Brad Allen has an awesome collection of Chevrolet factory pictures that he has set up from film strips.

Check them out!

Lots of work on Brad's part ... pure enjoyment (and references) for you!

Big Thanks!

THANKS!

For helping keep this great
old truck web site
on the Internet for

over 30 years!

and not clogged down
with Ads!


Again, thanks!

Previous Thread
Next Thread
Print Thread
#848808 05/04/2012 1:08 PM
Joined: Nov 2011
Posts: 139
5
Shop Shark
Shop Shark
5 Offline
Joined: Nov 2011
Posts: 139
Getting ready to sandblast frame. Structurally it's all good but there are a couple areas with some extensive pitting and another few areas where the edge is thinned out. Wondering if I should try to build up then grind down the pitts/thin spots or use some sort of filler? Any suggestions would be welcome. Thanks. I plan on using POR15 for the finish.

Joined: Mar 2008
Posts: 3,750
J
'Bolter
'Bolter
J Offline
Joined: Mar 2008
Posts: 3,750
AFAIK POR-15 will NOT adhere correctly to plastic filler/bondo.

If the areas aren't structural you might be able to lead solder them although i'm not sure if the POR will stick to that either.....

You could try a practice run on an old piece of scrap metal first.


1950 Chevy Advance Design 3100 in Scotland
In the Stovebolt Gallery
More pix on Flickr.
I've definately got this truck thing in my blood ... my DNA sequence has torque settings
"Of all the small nations of this earth,perhaps only the ancient Greeks surpass the Scots in their contribution to mankind" Winston Churchill.
Joined: Jun 2001
Posts: 793
T
Bondo Artiste
Bondo Artiste
T Offline
Joined: Jun 2001
Posts: 793
After repairs and filler application after they are primed por 15 should adhere just fine. Call the Por 15 service line and ask them about primers that work well with Por 15.


~ Phillip
1949 GMC Suburban - 10 year project
1952 Pontiac Chieftain Convertible straight 8 hydramatic
1945 GMC half ton truck - Driver- Sold 9-15-25
1946 Chevy COE - SOLD 1-5-26 BUH BYE CHEVY!
1959 GMC Half ton long bed NAPCO
Joined: Nov 2011
Posts: 139
5
Shop Shark
Shop Shark
5 Offline
Joined: Nov 2011
Posts: 139
Thanks for the input. I looked at the POR15 site and they have a thickened POR15 in tubes that works as a filler. Figure I'll use that for the smaller pits. Guess I'll see what's left after sandblasting and decide how to proceed with deeper pits and thin areas.


Moderated by  klhansen 