Click on image for the lowdown. 
====
| | | Forums66 Topics128,068 Posts1,055,881 Members48,428 | | Most Online14,466 Apr 26th, 2026 | | AD Chevy Trucks Over 6,000 pictures Brad Allen has an awesome collection of Chevrolet factory pictures that he has set up from film strips. Check them out!
Lots of work on Brad's part ... pure enjoyment (and references) for you!
| | THANKS!
For helping keep this great
old truck web site
on the Internet for over 30 years! and not clogged down with Ads! Again, thanks! | | | | Joined: Jun 2014 Posts: 152 'Bolter | | 'Bolter Joined: Jun 2014 Posts: 152 | while rebuilding my 235 i decided to do a spot of diy chroming. 235 engine diy chrome total cost was around 1000usd including a buffing machine and all the chemicals which isnt bad considering local prices to get one part chromed was around 250 a part and i have plenty of chemicals left to do any number of other things hardest part to do by far was the sump draft tube as it was impossible to degrease the inside so i had to seal both ends first. anyway i think it came out nice especially the oil filter housing and the theromostat inlet casting I chrome plated:- cooling fan Thermostat casting fuel filter housing manifold clamps throttle linkages fuel pump top sump draft tube oil filter housing various bolts and some other bits and pieces stuff that was easier and cheaper to buy already plated like the rocker cover and timing gear cover I just bought off the shelf
Last edited by Drmike; 03/09/2015 4:52 AM.
| | | | | Joined: Oct 2006 Posts: 9,671 'Bolter | | 'Bolter Joined: Oct 2006 Posts: 9,671 | As they used to say when I was a lad, if it don't go, chrome it. But all kidding aside Mike, that is cool. Is that a Caswell chrome kit you were using? I see you had to do 1/2 at a time with the draft tube, you didn't mention the side cover, did you find that already chromed or did you do that half at a time also? And how did that work out, was there a parting line where you did the other half? I see also that you did copper, did you do nickle over the copper then the chrome, i.e., triple chrome? I'm assuming you buffed, then copper, buffed again then nickle before the final chrome? I understand that 90% of the job is buffing, but about how long did it take for the actual plating baths? Reason I'm so full of questions is I've got a couple of Caswell kits on the shelf and have been just plane scared to use them without knowing how to dispose of the chemicals after they peter out. I'll bet you had some real issues in Japan, aren't they super fussy about that sort of thing?
Thanks for the pix. What's that open wheel car we see in the back ground??
Denny Graham Sandwich, IL
Denny G Sandwich, IL
| | | | | Joined: Aug 2012 Posts: 1,214 Shop Shark | | Shop Shark Joined: Aug 2012 Posts: 1,214 | Looks real good. I wondered what my Blue Flame 235 would look like chromed and based on your pics and craftmanship it would look good  Dave | | | | | Joined: Feb 2000 Posts: 987 'Bolter | | 'Bolter Joined: Feb 2000 Posts: 987 | DrMike looks good I too would like to know more details. I see you have a 8" buffer in the back ground. What did you use for polishing compound? Would you be willing write a Tech tip for all the rest of us??????
Thanks again for posting the pics. Looking forward to hearing more about this.
Brian Moore 1949 3100 5 window Deluxe "Today is better than yesterday, but not as good as tomorrow" | | | | | Joined: Jun 2014 Posts: 152 'Bolter | | 'Bolter Joined: Jun 2014 Posts: 152 | hi Denny, Is that a Caswell chrome kit you were using? I see you had to do 1/2 at a time with the draft tube, yes it is. draft tube was impossible to clean of oil inside so i plugged the ends of the main body then did that first with the outlet sticking out the tank then inverted it to do the outlet, after taking off the plugs. that way i didnt get any chemicals washing out the oil from inside. with buffing no join line is visiable as i gave everything a thick plate so plenty to polish flat. you didn't mention the side cover, did you find that already chromed yes I see also that you did copper, did you do nickle over the copper then the chrome, i.e., triple chrome? I'm assuming you buffed, then copper, buffed again then nickle before the final chrome? I understand that 90% of the job is buffing, but about how long did it take for the actual plating baths? Reason I'm so full of questions is I've got a couple of Caswell kits on the shelf and have been just plane scared to use them without knowing how to dispose of the chemicals after they peter out. I'll bet you had some real issues in Japan, aren't they super fussy about that sort of thing?  yes polishing the parts prior to plating is 95% of the work. get it mirror then plate then buff it back to mirror. i didnt use chrome i used `copy chrome` which is actually cobalt. so no safety or disposal issues to deal with. i flash copper plated first for 40 mins then copy chrome plate for 90 mins. most important step is to 100% degrease before plating. but its definately addictive lol.. good luck! What's that open wheel car we see in the back ground?? yep a F3 car and a Reynard F3000 mecars ...500bhp and only 500kg....terrifying! 
Last edited by Drmike; 03/10/2015 2:14 AM.
| | | | | Joined: Jun 2014 Posts: 152 'Bolter | | 'Bolter Joined: Jun 2014 Posts: 152 | i used the white compoud.
i found that it was quite easy to prep parts if i simply followed the following-
1. orbital sander with 80 grit 2. orbital sander with 120 grit 3. orbital sander with 180 grit 4. buffing machine with white compound 5. kitchen sink and dish washing liquid to wash off most of oils 6. 20 - 30 mins in hot degrease tank 7. plate flash copper 8. plate copy chrome (cobalt) 9. buffing machine polish
this gave me a good mirror finish and no scratches
after plating its usually necessary to go back to the buffer to flatten any rough plate surface and final polish especially if you do a think plate.
with copy chrome (cobalt) you dont have to use copper first on steel but i found it was better to do so as you can see when or if you polish through the cobalt plate when you do final polish.
to plate the zinc alloy parts you need to plate copper first
Last edited by Drmike; 03/10/2015 2:17 AM.
| | | | | Joined: Jun 2014 Posts: 152 'Bolter | | 'Bolter Joined: Jun 2014 Posts: 152 | my plan is to chrome plate the pedals and the gear lever (shifter) next...i think theres not much left after that to chrome lol
| | | | | Joined: Oct 2006 Posts: 9,671 'Bolter | | 'Bolter Joined: Oct 2006 Posts: 9,671 | Beautiful car Mike. I drove midgets here in the states for a while and had a few chances to get into the USAC Sprint car we had for awhile, which has similar power to weight ratios to that formula car, was really fun to drive. Built a Pitts special biplane some years back and that was mild in comparison with it's 160hp and 750lb. weight but still fun to fly. That almost felt like you just strapped a set of wings on your back and all you had to do was think and it did what you wanted it to. Thanks for the update on the copy chrome, that's the kit I've got on the shelf. Sure looks good. So there isn't a nickle base for the cobalt. That's obviously a much thicker deposit than chrome as it, really needs the nickle for protection since the chrome is deposited so thin. Can you get the copper thick enough with their kit's to cover scratches or blemishes such as those often found in the zinc castings? Sort of like you would use a primer/surfacer buildup in painting.
Denny Graham Sandwich, IL
Denny G Sandwich, IL
| | | | | Joined: Sep 2006 Posts: 2,393 Shop Shark | | Shop Shark Joined: Sep 2006 Posts: 2,393 | Very interesting. I was not aware this system is available. I am curious if you experienced any fuming condition that was hard to ventilate. We used to called them "heavy fumes" at work for lack of a better description. For those interested as I am, here is a Caswell link with a very informative half hour video of instruction. http://www.caswellplating.com/elect...ing-kits/triple-chrome-plating-kits.htmlAnd as an old SCCA guy, kudos on the immaculate F3.
Drew
| | | | | Joined: Oct 2006 Posts: 9,671 'Bolter | | 'Bolter Joined: Oct 2006 Posts: 9,671 | Ask then how you dispose of the chemicals when they are used up Drew, a few years ago when I bought my kits from them they couldn't give me an answer other than dispose of it properly, which I took to mean a has mat facility......BIG BUCKS.
Denny G
Denny G Sandwich, IL
| | | | | Joined: Jun 2014 Posts: 152 'Bolter | | 'Bolter Joined: Jun 2014 Posts: 152 | Can you get the copper thick enough with their kit's to cover scratches or blemishes such as those often found in the zinc castings? Sort of like you would use a primer/surfacer buildup in painting. yup the flash copper can be put on thick and used as a filler sanding it down to fill in marks in the surface and polishing easily before going to cobalt. if really pitted you can also plate with acid copper after a quick protective flash copper which will enable you to add a really thick `filler` cu layer quicker if needed
Last edited by Drmike; 03/11/2015 8:59 AM.
| | | | | Joined: Sep 2006 Posts: 2,393 Shop Shark | | Shop Shark Joined: Sep 2006 Posts: 2,393 | Denny, With any toxic chemical it's a problem for sure. But, we had this old adage at work. "The solution to pollution is dilution". Quaint, but true and is how even on a large scale it is done, of course with other added neutralizers. Water is the universal solvent. Providing you are not disposing of a 50 gallon drum of chromate solution, and if you want,just keep cutting it with water. It would be nice if you had a pH meter, but likely you don't, so buy acid/base papers from a pool supply and as you dilute keep checking until it's neutral. You can decide what to do with it then.
Last edited by DrewP; 03/11/2015 5:13 PM.
Drew
| | | | | Joined: Oct 2006 Posts: 9,671 'Bolter | | 'Bolter Joined: Oct 2006 Posts: 9,671 | Thanks Mike, you've given me a bit of a boot in the hind quarter to get going and try out my kits. Got the 4.5 gallon sizes so I should be able to do some fairly decent sized parts.
Wonder if I could use a long plastic tray rather than the 5 gallon bucket for a tank so I could do a long narrow piece like a side cover?
Denny G
Last edited by Denny Graham; 03/11/2015 5:14 PM.
Denny G Sandwich, IL
| | | | | Joined: Sep 2006 Posts: 2,393 Shop Shark | | Shop Shark Joined: Sep 2006 Posts: 2,393 | Denny, maybe use a plastic rain gutter section or slice a 8" diameter sewage pipe in half and add caps? Just thought.
Drew
| | | | | Joined: Jun 2014 Posts: 152 'Bolter | | 'Bolter Joined: Jun 2014 Posts: 152 | hi denny yup this is what i had to do for the cooling fan. it wouldnt fit inside the 4.5 gallon drum so i used a larger box.
for the gear shift im going to use a bit of drain pipe, vertical, bottom end capped and move the shifter gradually down it as it plates
probably something similar would work well for a side cover to get the coverage you can `move` the part over two plates in the bottom of a shallow tray
or you could simply use the 4.5 gallon drum and plate one half at a time with a thick enough plate you can easily (with a machine) buff out the join/overlap
once you start plating you end up wandering around looking for things to plate - its kinda addictive lol
Last edited by Drmike; 03/12/2015 12:07 AM.
| | | | | Joined: Oct 2006 Posts: 9,671 'Bolter | | 'Bolter Joined: Oct 2006 Posts: 9,671 | Good ideas for the loooong tanks. And I'm sure it is, addictive that is, every time I find something good it always seems to end up taking over every spare minute of my time. Then before you know it, your plating zinc and nickle.
Thanks for all the tips, should really help some of the guys that want to dress up their Stovebolts. It was kind of a surprise hearing it from someone half way round the world.
dg
Denny G Sandwich, IL
| | | | | Joined: Jun 2014 Posts: 152 'Bolter | | 'Bolter Joined: Jun 2014 Posts: 152 | update: for the gear shifter I just used a bucket and did half at a time overlapping the `join`
with a thick 1hr plate it was easy to buff away the `join` in the plating so you could never tell it was plated in two halfs rather than at once
in future with long items im not sure id bother using fancy tanks, just overlapping seems to work ok
other thing i learnt the hard way is if you plan on doing heavy machine polishing/buffing its often better to plate (copychrome) direct to steel rather than Cu first. the reason is the copychrome blisters off the cu if it gets hot under the buffer.
Last edited by Drmike; 06/24/2015 1:57 AM.
| | | | | Joined: Dec 2003 Posts: 2,953 'Bolter | | 'Bolter Joined: Dec 2003 Posts: 2,953 | Denny speaking of Pitts Specials did you ever fly a radial powered Pitts? I flew in one. It has the Russian or Polish round engine or perhaps the Chinese version we have in the Nanchang. That was fast and the roll rate so fast you could 720 in one direction and snap into a 720 in the other and never knew you had! Sorry off topic here> | | | | | Joined: Oct 2006 Posts: 1,847 'Bolter | | 'Bolter Joined: Oct 2006 Posts: 1,847 | dilution is NOT the answer to pollution. Its the answer we give ourselves to pacify our conscience. Not creating the pollution in the first place is the correct answer. It reminds me of smokers toothpaste. The guy is all racked up, near death from smoking, but hey his teeth are pretty. Here in Washington state, there is basically no freshwater locations that pregnant women or children, can eat the fish from, and only a small amount for a healthy adult. I really like my old truck, but it is such an environmental pig. I can justify taking it out for a couple of short jaunts once a week or so, but as a daily driver I feel it would be rather irresponsible. This however is MY OPINION, feel free to agree or not. Sorry if I got a little off the topic, but at some point we as a species (human) will have to confront this issue head on. | | |
| |