Originally Posted by 78buckshot
RLB, did you use a catalyst in the acrylic enamel or is it straight air dry? It will be important to let the finish cure as long as possible, so you are not plugging up the abrasive paper with gummy deposits, the paint will cut easier and smoother if it is fully cured. I wet sanded some acrylic urethane and buffed, no clear before or after.


I used the dealer supplied catalyst. No gummy deposits while wet sanding. That part of operation went really well. Buffing seems to be an aquired skill . I 'm not seeing any sand scratches, just buffing swirls with less than good shine.


1966 C-10 Short Stepside
HiPo
Step-by-step ~ and on-going resto build
in the Project Journals