The Stovebolt.com Forums Home | Tech Tips | Gallery | FAQ | Events | Features | Search
Help is a click away!

VEHICLE
INFORMATION
KITS


at the

GM Heritage Center
All the details are here.

Searching the Site - a click away
click here to search
New here ??? Where to start?
Click on image for the lowdown. Where do I go around here?
====
Who's Online Now
0 members (), 118 guests, and 3 robots.
Key: Admin, Global Mod, Mod
Forum Statistics
Forums66
Topics128,186
Posts1,057,320
Members48,469
Most Online14,466
Apr 26th, 2026
Step-by-step instructions for pictures in the forums
Brad Allen's photos

AD Chevy Trucks

Pictures galore
Over 6,000 pictures

Brad Allen has an awesome collection of Chevrolet factory pictures that he has set up from film strips.

Check them out!

Lots of work on Brad's part ... pure enjoyment (and references) for you!

Big Thanks!

THANKS!

For helping keep this great
old truck web site
on the Internet for

over 30 years!

and not clogged down
with Ads!


Again, thanks!

Previous Thread
Next Thread
Print Thread
Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
Wanted to see what the opinions were here on the best way to finish this seam. Originally leaded of course. On some sites it is recommended to re-lead this seam, stating that body filler doesn't hold up and will crack. Others have said they use a filler with fibers in it for the roughing in of the join with a skim coat of body filler to finish up with.
I have to admit I've never tried using lead solder before.
Thanks John

Joined: Aug 2005
Posts: 6,378
T
Ex Hall Monitor
Ex Hall Monitor
T Offline
Joined: Aug 2005
Posts: 6,378
If the surface is properly prepared I see no reason why body plastic wouldn't bond well. I'm not familiar with the seam so there may be more at play than I'm aware of.


Save a life, adopt a senior shelter pet.
The three main causes of blindness: Cataracts, Politics, Religion.
Name your dog Naked so you can walk Naked in the park.
Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
I wouldn't think there would be a lot of flex in this area. Be the leaded seam right above the cowl vent on the passenger side.

John

Joined: Dec 2000
Posts: 3,399
D
Gas Pumper
Gas Pumper
D Offline
Joined: Dec 2000
Posts: 3,399
The builders of these trucks didn't build them to have any flex. The places where there is lead is simply because that was the bondo of its day. We now have fillers that completely exceed any expectation the original designers had for these trucks. If a person wanted to be sure, just weld the seam. I have done several of these with plastic and its just not a problem.


Deve

1950 Chevy 3100 Deluxe Cab
1950 Chevy 3100 Standard Cab
In the Stovebolt Gallery
The Think Tank
More info and tips at Deve's Technet
Joined: Sep 2001
Posts: 29,270
Bubba - Curmudgeon
Bubba - Curmudgeon
Joined: Sep 2001
Posts: 29,270
There is not a lot of flex in that location.
It is just a joint. Lead made an excellent metal to metal joint/seal.

On GMC truck cabs, in 1954/55, that joint was made low in that window frame with a brass/bronze seal/weld and it was not smoothed over with filler.

Have you removed the lead?

Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
No I haven't removed the lead yet. On the driver's side I was able to put in a panel without getting into the joint area. But on the passenger's side I think I'll have to go with a whole panel to correct past problems.

John

Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
I'm thinking about using something like Duraglass for most of the filling and skim it with regular body filler to finish. Or would it be better to smooth the finish coat with something like "Icing"?
Question is, do I apply the filler straight to the metal after roughing it with an 80 grit disc as we use to do it or prime it with epoxy primer and then the filler as many say to do now??

John

Joined: Dec 2000
Posts: 3,399
D
Gas Pumper
Gas Pumper
D Offline
Joined: Dec 2000
Posts: 3,399
Ten years ago, it was etching primer that was the first step. But now its epoxy primer. I can see why too. Its much more durable and sticks better. No doubt epoxy primer first. Rage Gold is just fine for the filler step. The rule is anything in the 1/8" depth area filler is appropriate. Never fill with any filler deeper than 1/8 inch. Once you have it VERY close but its still a bit low, Polyester filler (glaze) is used. The idea is epoxy first, filler, urethane high build primer.. usually this makes the surface high enough with no need for glaze.

What invariably happens is, you sand in some places down to the epoxy. So lets say you are a Clutz like me and you sand to the bare metal in some places after all of this work. That's the beauty of following correct auto body standards. The next step after doing all of the previous is Epoxy Sealer which you don't sand, then topcoat.

So, short answer is Epoxy, then filler, then 80 grit, then 220 grit. It may still be a little low, so then high build primer and/or polyester glaze, then 400 grit. Once you really like the feel of it, sealer then topcoat. I never use air tools or anything power. All sanding for the entire truck is done by hand. You learn the touch and feel aspects which are so important better that way.

When I started all of this, I purchased all of the fancy power tools for sanding. Spent a little time with some of the local professionals and now I am convinced that the tactile touch and feel of sanding by hand is far better. If you go to one of the accident specialist body shops, they will beg to differ due to the time savings. Restorers who really care about the end result do it all by hand. Evercoat's Rage Gold is my filler of choice.


Deve

1950 Chevy 3100 Deluxe Cab
1950 Chevy 3100 Standard Cab
In the Stovebolt Gallery
The Think Tank
More info and tips at Deve's Technet
Joined: Dec 2000
Posts: 3,399
D
Gas Pumper
Gas Pumper
D Offline
Joined: Dec 2000
Posts: 3,399
Forgot.. make sure the bare metal is cleaned with metal prep. DX330 is PPGs answer. I use that. Its a very important step.


Deve

1950 Chevy 3100 Deluxe Cab
1950 Chevy 3100 Standard Cab
In the Stovebolt Gallery
The Think Tank
More info and tips at Deve's Technet
Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
I have to admit, I can't feel the highs and lows as well as I'd like. I usually use Klean-Strip wax and grease remover to clean the metal surface before painting ect.... I have even used lacquer thinner to wipe down new metal that has been very oiled before. Seems to remove the oil film faster. Then clean it with wax and grease remover then.

John

Joined: Aug 2005
Posts: 6,378
T
Ex Hall Monitor
Ex Hall Monitor
T Offline
Joined: Aug 2005
Posts: 6,378
You want to use your preferred wax and grease remover BEFORE you do any sanding. Otherwise you can drive contaminants into the surface you are working on. Then follow up with another cleaning before paint. Remember to put it on wet and wipe it off before it dries.


Save a life, adopt a senior shelter pet.
The three main causes of blindness: Cataracts, Politics, Religion.
Name your dog Naked so you can walk Naked in the park.
Joined: Mar 2010
Posts: 10,310
5
Renaissance Man
Renaissance Man
5 Offline
Joined: Mar 2010
Posts: 10,310
Originally Posted by Whitelightning
I have to admit, I can't feel the highs and lows as well as I'd like. I usually use Klean-Strip wax and grease remover to clean the metal surface before painting ect.... I have even used lacquer thinner to wipe down new metal that has been very oiled before. Seems to remove the oil film faster. Then clean it with wax and grease remover then.

John
Have you ever tried it with a thin jersey glove? It makes no logical sense to me why it works, but I was amazed at how much better I can feel the high and low spots with one.


1952 5-window - return to "as built" condition | 1950 3100 with a 235 and a T-5 transmission
Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
Never heard tell of that method. I have heard people say use a piece of tissue paper between your palm and the panel. I usually try a guide coat of paint.

John

Joined: Aug 2005
Posts: 6,378
T
Ex Hall Monitor
Ex Hall Monitor
T Offline
Joined: Aug 2005
Posts: 6,378
A couple of "tricks" I learned long ago in another life when I went to body & fender trade school then worked in the trade for a few years. When you run your hand over a panel to "read" it, lay your hand full flat against the panel. Start the read on an unmolested part of the panel then move your hand over the worked part of the panel to an unmolested area on the other side of the worked area. Move your hand forward and back in the direction your fingers are pointing, not side to side. It helps to wear cotton gloves or put a rag between your hand and the panel if you're having difficulty getting a good read of the panel. I found it also helped sometimes to close my eyes if I was having trouble getting a good read.

Last edited by Tiny; 12/02/2013 3:08 PM.

Save a life, adopt a senior shelter pet.
The three main causes of blindness: Cataracts, Politics, Religion.
Name your dog Naked so you can walk Naked in the park.
Joined: Jul 2011
Posts: 785
M
'Bolter
'Bolter
M Offline
Joined: Jul 2011
Posts: 785
The other option would be to flatten out the stepped flange, trim and butt weld the cowl piece in for a no filler (less filler?) repair. Many of these lapped and leaded joints were done at the factory for speed of assembly more than anything else. Get rid of the lap, it gets rid of the need for filler. Here's some similar sample "de-leading" and seam removal...


http://www.trifive.com/forums/showpost.php?p=357820&postcount=45


http://www.trifive.com/forums/showpost.php?p=360642&postcount=58



Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
That is an idea. Might have to rework the top of the panel a little to match up.

John

Joined: Jul 2013
Posts: 224
W
Shop Shark
Shop Shark
W Offline
Joined: Jul 2013
Posts: 224
I just did this ....used a small torch heated up the lead wiped off with rag while hot ....drilled out the welds .... drilled
1/4 " holes in new cowl ....welded in new cowl ....don't forget to drill holes in flange at door for welding ,...bondo fit the bill .... primed & painted yesterday I like it ....John Deere blitz black ....


" STUCK IN THE '50'S "
Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
Thanks all, sounds like I can get along with a good grade body filler then. I think I'm going to order the outer cowl, floor pan, cab mount and rocker panel. I'll make the inner to outer and the inner cowl myself.
John

Joined: Jun 2009
Posts: 1,596
4
'Bolter
'Bolter
4 Offline
Joined: Jun 2009
Posts: 1,596
If you want to put a filler on the top that is flexible, use paintable autobody caulking from you autobody supply store. Then you can paint right over it and it still stays a little flexible.


1946 GMC Pickup - S-10 Frame, 455 Buick, TH400, original patina.

My 46 GMC on Photobucket
Joined: Dec 2001
Posts: 1,248
W
'Bolter
'Bolter
W Offline
Joined: Dec 2001
Posts: 1,248
I've used the body chalk on flexible seams before. The only problem... The chalk will flex more than the paint does. Then you see white cracks in the paint. Probably wouldn't be a problem in this case, because I don't believe there is much flex at that area of the cab.

John


Moderated by  klhansen 

Link Copied to Clipboard
Home | FAQ | Gallery | Tech Tips | Events | Features | Search | Hoo-Ya Shop
Powered by UBB.threads™ PHP Forum Software 8.0.0