Plating pot is probably the hardest to do. Stripping off the old plating first. Then depending on how bad it is it takes many,many layers of copper to fill the holes in. Each time after plating copper it is polished again . Process is done over and over till it come out smooth. Then nickel and chrome after that. Check out their work before putting the money down.
Yikes! I got my gmc grille bars, hood emblem, side emblems, and the model hood callouts all rechromed for $1100. Canadian. One of my model callouts (9430) has pitting and they asked me if I wanted it perfect. No, I said.
Cheap as possible? Not that either.
Their mid range standard chrome options came out pretty good for me.
Alberta Plating in Calgary, Ab did mine.
1970 Chevrolet C10 Grandpa's -- My first truck -- In progress to shiny Follow the build in the Project Journal 1950 Chevrolet 1-Ton Dually "Ole Red Girl" In the Stovebolt Gallery More pictures here 1951 GMC 9430 1 ton dually--Shiny! | 1972 Chevrolet C20- Rusty- the puzzle box lid for the C10 | 1962 AMC Rambler American- my wife's Parts trucks- 1951 GMC 9300 | 1951-GMC 9430 | 1951- Chevrolet 1300