on the Internet for over 30 years! and not clogged down with Ads! Again, thanks! | | | | Joined: Oct 2001 Posts: 3,458 Extreme Gabster | | Extreme Gabster Joined: Oct 2001 Posts: 3,458 | Well, all of the temperature sending units use brass fittings with no problems. It may be that the corrosion of the iron is normal or caused by cavitation from the water pump. Try a bit of teflon tape on the threads, maybe that would help? Or you could switch to brass elbows.