Click on image for the lowdown. 
====
| | |
1 members (tclederman),
94
guests, and
4
robots. | | Key: Admin,
Global Mod,
Mod | | | Forums66 Topics128,181 Posts1,057,185 Members48,465 | | Most Online14,466 Apr 26th, 2026 | | AD Chevy Trucks Over 6,000 pictures Brad Allen has an awesome collection of Chevrolet factory pictures that he has set up from film strips. Check them out!
Lots of work on Brad's part ... pure enjoyment (and references) for you!
| | THANKS!
For helping keep this great
old truck web site
on the Internet for over 30 years! and not clogged down with Ads! Again, thanks! | | | | Joined: May 2006 Posts: 8,351 'Bolter | | 'Bolter Joined: May 2006 Posts: 8,351 | Calling it "copper-nickel" might be a little misleading. The alloy used is actually copper-nickel-iron. It takes double flares just fine, as Dave states, much easier than paint steel.
Bill Burmeister | | | |
Entire Thread
|
Copper-nickel brake lines & galvanic corrosion, anyone?
| Mikestem | 02/24/2015 6:52 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Jim Sears | 02/24/2015 8:16 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| diseasel | 02/24/2015 9:10 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| thoroco | 02/24/2015 9:38 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| LONGBOX55 | 02/24/2015 10:18 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Achipmunk | 02/24/2015 10:29 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| jockbolter50 | 02/25/2015 9:47 AM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| cmayna | 02/25/2015 3:51 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| DennisM | 02/25/2015 4:29 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Mikestem | 02/25/2015 7:49 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Hotrod Lincoln | 02/25/2015 11:06 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Mikestem | 02/27/2015 2:08 PM | |
| |
| |