on the Internet for over 30 years! and not clogged down with Ads! Again, thanks! | | | | Joined: Nov 2010 Posts: 123 'Bolter | | 'Bolter Joined: Nov 2010 Posts: 123 | I always thought copper-nickle was best used for fuel line application, or anything with a "single flare to brass." I could be wrong but my guess is that copper would fatigue more under brake line pressure and higher torqued connections with steel. | | | |
Entire Thread
|
Copper-nickel brake lines & galvanic corrosion, anyone?
| Mikestem | 02/24/2015 6:52 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Jim Sears | 02/24/2015 8:16 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| diseasel | 02/24/2015 9:10 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| thoroco | 02/24/2015 9:38 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| LONGBOX55 | 02/24/2015 10:18 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Achipmunk | 02/24/2015 10:29 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| jockbolter50 | 02/25/2015 9:47 AM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| cmayna | 02/25/2015 3:51 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| DennisM | 02/25/2015 4:29 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Mikestem | 02/25/2015 7:49 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Hotrod Lincoln | 02/25/2015 11:06 PM |
Re: Copper-nickel brake lines & galvanic corrosion, anyone?
| Mikestem | 02/27/2015 2:08 PM | |
| |
| |