I can grab a pic of the can later today. It is what the body guy who helped me spray uses when he has small touch up to do.
I just spoke with the liner people. He thinks the primer didn't sand the same way as the high build and had too glossy of a finish causing the balling. It was one of the things I did notice when we were final blocking, but I never thought twice about it. It had been on for 5 to 6 days prior to finish sanding. Many of these areas I will be able to sand down and re shoot. It has such a long flash time it is self leveling so I am hopeful I can get things looking good?
I will be very happy with the finished product if I can straighten this problem out. It is going to be super rugged I can tell and it will take another day or two to fully cure.
Last edited by Ferris Bueller; 08/14/2023 3:51 PM.