I would die grind, out the crack into a V .Drill hole at end of crack then fill.
https://www.muggyweld.com/ this melts at very low heat and is super strong and can be filed smooth. I have used this with great success,on many cracks ,and it has never re cracked . Applies like solder, flows into crack perfectly.