Yup you're right Joe, makes it easier though if you'd been following the thread for a couple of years.
Originally posted by red58:
US Tremclad/Rustoleum dealers - same product
the problem I'd have with Brightside is Interlux paints are designed and intended for use on wood/fiberglas, tho' maybe it doesn't make any difference
Bill I think it is OK for all surfaces judging by the Product Data Sheet:
Preparation
BARE FIBERGLASS: In Good Condition Begin by scrubbing well using soap and water and a stiff brush. Rinse with fresh water and allow to dry. Wipe a small area with a clean rag that has been wetted with Fiberglass Solvent Wash 202. While the surface is still wet, wipe with a clean, dry rag. Continue this process until the entire surface has been cleaned. Sand with 220-320 grade (grit) paper. Remove sanding residue. In Poor Condition Clean as above. Sand with 80 grade (grit) paper. Apply Brightside Primer.
BARE WOOD: Sand surface, wipe clean. Apply Brightside Primer. Sand surface, wipe clean.
BARE METAL: Sandblast or grind, remove sanding residue. Immediately apply Viny-Lux Primewash 353/354 thinned 25% with Viny-Lux Solvent 355. Allow to dry for 1-24 hours. Apply one coat of Epoxy Barrier-Kote 404/414.
CLEAR EPOXY: Clean as for Bare Fiberglass above. Sand with 80 grade (grit) paper. Remove sanding residue. Apply one coat of Epoxy Barrier-Kote 404/414.
PREVIOUSLY PAINTED SURFACES: The surface must be clean and dry. Sand with 220-320 grade (grit) paper. Remove sanding residue.